Choosing the grade

304 or 316L: choose by chlorides

How to choose between 304 and 316L for coastal, chlorinated or disinfectant service, with pitting resistance, composition and grade comparisons.

Published 2026-11-13
304 or 316L: choose by chlorides · Cover

The rule in one line

One question decides it: whether the service environment contains chlorides. Coastal and Hong Kong/Macao outdoors, chlorinated water treatment, disinfectants and cleaning agents, sea mist and chemical-plant atmospheres — start those at 316L. Indoor atmospheres, fresh water and mild corrosion are 304’s ground as the general-purpose grade. The difference sits in the composition: 316L carries 2.0–2.5% molybdenum, 304 carries none, and molybdenum is the element that resists chloride pitting.

Pitting resistance and composition across the five stock grades

GradeSeriesChromium CrNickel NiMolybdenum MoPitting resistance
201200-series, low-nickel16.0–18.03.5–5.3—★★☆☆☆ (average; dry indoor)
304300-series austenitic18.0–20.08.0–10.5—★★★☆☆ (room-temperature atmosphere, fresh water, mild corrosion)
316L300-series Mo-bearing16.5–18.510.0–13.02.0–2.5★★★★★ (strong against chloride pitting)
430400-series ferritic16.0–18.0≤0.75—★★☆☆☆
409L400-series ferritic (Ti-stabilised)10.5–11.5≤0.50—★★☆☆☆ (atmospheric and mild corrosion)

Where 201, 430 and 409L fit

  • 201: dry indoor work — decorative tubing, signage, household hardware. Not for coastal outdoors, chloride cleaning, food or medical contact, or heating above 300 °C.
  • 430: nickel-free, magnetic and a good heat conductor; appliance back panels and magnetic trim are its ground. Avoid damp outdoors, deep drawing and parts that must take heavy weld distortion, and mind the 475 °C embrittlement range.
  • 409L: titanium-stabilised ferritic, oxidation resistant to about 815 °C, used for automotive exhaust systems and equipment flue pipes. For food or drug contact surfaces start at 304.

Which grade we quote in practice

Equipment doors, meter boxes and EV-charger housings for Hong Kong and Macao, and framed gratings of the outdoor and municipal kind, are quoted in 316L by default: where chlorides and hygiene requirements arrive together, its pitting resistance and extra-low-carbon welding behaviour both hold up. Kitchenware and catering equipment, food machinery housings, architectural decoration and appliance panels — the inland service cases — go to 304, whose welding and forming are balanced and whose thin wall can skip annealing.

Framed steel grating: this order was supplied in 316L and shipped in batches by item number
Framed steel grating: this order was supplied in 316L and shipped in batches by item number
What happens if 304 is used outdoors on the coast?

Chloride ions break down the passive film on the surface first: pitting starts as rust spots and shows up sooner on overlaps, weld roots and the crevices under seal rings. For coastal and Hong Kong/Macao outdoor parts we quote 316L by default, and where the drawing specifies another treatment we cost against the drawing.

Can 201 simply replace 304?

Yes for dry indoor parts where appearance is not critical. 201 substitutes manganese and nitrogen for part of the nickel, so its pitting resistance sits clearly below 304 and it is not recommended for damp or chloride-containing service. It work-hardens strongly and suits large-deformation forming, and the heat input has to be kept down when welding.

How do I confirm the batch that arrived really is 316L?

A mill test certificate can travel with the order. If you need an MTR to EN 10204 3.1, or third-party testing by SGS or BV, state it in the enquiry and we arrange it per order. When goods arrive, check grade and thickness and keep the certificate together with your own measurement records.

The full comparison of grade parameters, composition and mechanical ranges sits on Sheets & Grades. Send the service environment, thickness, dimensions and quantity through Contact, and sales issue a numbered quotation costed against the market on the day you order.

Other articles in this section

The National Standard for Testing Pitting Corrosion of Stainless Steel Is Renewed: GB/T 17897-2026
Choosing the gradePublished 2026-11-24

The National Standard for Testing Pitting Corrosion of Stainless Steel Is Renewed: GB/T 17897-2026

Since 1 Nov 2026, GB/T 17897-2026 "Corrosion of metals and alloys—Corrosion test for pitting corrosion" is in force, fully replacing two 2016 standards. This article covers three things: what changed, what the standard does and does not govern, and what it means when you buy stainless steel. The official screenshots lead the article.

WhatsApp

Get a quote / leave a message

Submitting issues a request number right away, and a colleague picks it up and follows up during working hours; messages sent overnight or at weekends join the same queue and are handled first once we are back.

Need to add an email, a city or sample details? (open the full form), or .